Waya Constantan fun Sampling Resistor jẹ́ alloy copper-nickel tí ó sábà máa ń ní 55% Copper àti 45% Nickel. Ohun pàtàkì rẹ̀ ni resistance rẹ̀ tí ó dúró ṣinṣin lórí ọ̀pọ̀lọpọ̀ iwọn otutu. A tún ń pè é ní Alloy 294, Nico, MWS-294, Cupron, Copel, Alloy 45, Neutrology, Advance, CuNi 44, CuNi 44, CN49. Àwọn ìwọ̀n mìíràn ti alloy nickel bàbà ni a rí bí a ṣe ń sọ yìí: CN5, CuNi2,A60, Alloy 60, Alloy 60, MWS-60, Lohm, HAI-60, CuNi 6, Alloy 260, Nickel Alloy 60, CN10, CuNi10, CN15, A30, Alloy 30, CuNi23, Alloy 30, MWS-30, HAI-30, Alloy 230, Nickel Alloy 30, CN 30, CuNi1, CuNi15, CuNi30


Àlàyé Ọjà

Awọn ibeere ti a maa n beere nigbagbogbo

Àwọn àmì ọjà

Tita Taara Tita Ile-iṣẹ Cuni44 Resistance Alloy Ti a Lo Lati Ṣe Awọn Ohun elo Okun Thermocouple


Waya Constantan fun Sampling Resistor jẹ́ alloy copper-nickel tí ó sábà máa ń ní 55% Copper àti 45% Nickel. Ohun pàtàkì rẹ̀ ni resistance rẹ̀ tí ó dúró ṣinṣin lórí ọ̀pọ̀lọpọ̀ iwọn otutu. A tún ń pè é ní Alloy 294, Nico, MWS-294, Cupron, Copel, Alloy 45, Neutrology, Advance, CuNi 44, CuNi 44, CN49.
Awọn ipele miiran tialloy nickel bàbàÀwọn wọ̀nyí ni CN5, CuNi2
A60, Alloy 60, Alloy 60, MWS-60, Lohm, HAI-60, CuNi 6, Alloy 260, Nickel Alloy 60, CN10
CuNi10, CN15
A30, Alloy 30, CuNi23, Alloy 30, MWS-30, HAI-30, Alloy 230, Alloy Nickel 30, CN 30
CuNi1, CuNi15, CuNi30
Ti o ba ni ibeere tabi ibeere eyikeyi, jọwọ jọwọ kan si wa ni ọfẹ.

Àwọn Ohun Ànímọ́/Ìpele CuNi1 CuNi2 CuNi6 CuNi8 CuNi10
Iwọn otutu Iṣẹ Ti o pọju (º C) 200 200 200 250 250
Agbara resistance ni 20º C (Ω mm2/m) 0.03 0.05 0.1 0.12 0.15
Ìwọ̀n (g/cm 3) 8.9 8.9 8.9 8.9 8.9
Ìgbékalẹ̀ Ìgbóná (α × 10 -6 /º C) < 100 < 120 < 60 < 57 < 50
Agbára ìfàyà (Mpa) 210 220 250 270 290
EMF vs Cu (μ V/º C) (0 ~ 1000º C) -8 -12 -12 -22 -25
Ààyè Yíyọ́ Tó Súnmọ́ (º C) 1085 1090 1095 1097 1100
Àwọn Ohun Ànímọ́/Ìpele CuNi14 CuNi19 CuNi23 CuNi30 CuNi44
Iwọn otutu Iṣẹ Ti o pọju (º C) 300 300 300 350 400
Agbara resistance ni 20º C (Ω mm2/m) 0.2 0.25 0.3 0.35 0.5
Ìwọ̀n (g/cm 3) 8.9 8.9 8.9 8.9 8.9
Ìgbékalẹ̀ Ìgbóná (α × 10 -6 /º C) < 30 < 25 < 16 < 10 < -6
Agbára ìfàyà (Mpa) 310 340 350 400 420
EMF vs Cu (μ V/º C) (0 ~ 1000º C) -28 -32 -34 -37 -43
Ààyè Yíyọ́ Tó Súnmọ́ (º C) 1115 1135 1150 1170 1200