| Ni | Mn | Fe | Si | Cu | Òmíràn | Ìtọ́sọ́nà ROHS | |||
| Cd | Pb | Hg | Cr | ||||||
| 23 | 0.5 | - | - | Bọ́lù | - | ND | ND | ND | ND |
Àwọn Ohun Èlò Ìdánilẹ́kọ̀ọ́ Mẹ́kínẹ́ẹ̀kì
| Iṣẹ́ Ìtẹ̀síwájú Tó Pọ̀ Jùlọ | 300ºC |
| Agbara resistance ni 20ºC | 0.30ohm mm2/m |
| Ìwọ̀n | 8.9 g/cm3 |
| Ìgbékalẹ̀ Ooru | 16 (Pupọ julọ) |
| Aaye Iyọ | 1150ºC |
| Agbára ìfàyà, N/mm2 A ti fi ohun èlò pamọ́, Rọrùn | 350~420 Mpa |
| Agbára ìfàsẹ́yìn, N/mm2 Tí a yípo tútù | 380~840 Mpa |
| Gbigbe (anneal) | 25% (Pupọ julọ) |
| Igun (ti a yipo tutu) | 2% (Pupọ julọ) |
| EMF vs Cu, μV/ºC (0~100ºC) | -30 |
| Ìṣètò Mọ́kírófíkì | austeniti |
| Ohun ìní oofa | Kì í ṣe |
Awọn orukọ iṣowo CuNi23Mn:
Alloy 180, CuNi 180, Alloy 180, MWS-180, Cuprothal 180, Midohm, HAI-180, Cu-Ni 23, Alloy 380, Alloy Nickel 180
150 0000 2421